Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 7.7 - 8.7 g/cm³ Show Material materials with Dichte of 7.7 - 8.7 g/cm³ | Typical for Leaded Phosphor Bronze |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 110 - 130 GPa Show Material materials with Elastizitätsmodul of 110 - 130 GPa | Typical for Leaded Phosphor Bronze |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 75 - 81 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 75 - 81 [-] | |
Härte, Rockwell B | 23.0 °C | 86 - 98 [-] Show Material materials with Härte, Rockwell B of 86 - 98 [-] | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Zugfestigkeit | 23.0 °C | 625 - 730 MPa Show Material materials with Zugfestigkeit of 625 - 730 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Chemical properties
Property | Value |
---|---|
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Phosphor | 0.03 - 0.35 % Show Material materials with Phosphor of 0.03 - 0.35 % |
Zink | 0.3 % Show Material materials with Zink of 0.3 % |
Zinn | 3.5 - 4.9 % Show Material materials with Zinn of 3.5 - 4.9 % |