EN 1652 Grade CuZn39Pb2 H070

View suppliers (20)
Want to keep this datasheet? Save it now in your required format

Description

Material CuZn39Pb2, mat. No. CW612N, is an unhardenable wrought alloy. to the comparable make CuZn39Pb2, mat. No. 2.0380 acc. to DIN 17660 : 1983-12 applies: High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for the unleaded brass grade of the same Zn-content. Machinability is improved by Pb-addition. Corrosion resistance to water, several saline solutions and organic liquids is also lower than for unleaded alloys of the same zinc-content. Processing properties: warm forming: very good cold forming: unfavorable machinability: very good hard soldering: moderately soft soldering: very good TIG-welding: unfavorable burnishing: very good Application: For components in precision mechanics, machine and apparatus engineering as well as for circuit boards and clockwerks for watch industry.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.4 - 8.45 g/cm³

Show Material materials with Dichte of 8.4 - 8.45 g/cm³

Mechanisch

PropertyTemperatureValueComment

Elastizitätsmodul

20.0 °C

102 GPa

Show Material materials with Elastizitätsmodul of 102 GPa

Härte, Brinell

20.0 °C

70 - 170 [-]

Show Material materials with Härte, Brinell of 70 - 170 [-]

Härte, Vickers

20.0 °C

80 - 110 [-]

Show Material materials with Härte, Vickers of 80 - 110 [-]

Poissonzahl

20.0 °C

0.34 [-]

Show Material materials with Poissonzahl of 0.34 [-]

Schubmodule

23.0 °C

40 GPa

Show Material materials with Schubmodule of 40 GPa

Typical for Wrought Copper Brass

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

100.0 °C

2E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K

300.0 °C

2.1E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 1/K

Schmelzpunkt

875 - 1075 °C

Show Material materials with Schmelzpunkt of 875 - 1075 °C

Typical for Wrought Copper Brass

Spezifische Wärmekapazität

20.0 °C

377 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K)

Wärmeleitfähigkeit

20.0 °C

109 - 117 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 109 - 117 W/(m·K)

200.0 °C

134 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 134 W/(m·K)

Unlock all property charts

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

1.39E+7 - 1.40E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 1.39E+7 - 1.40E+7 S/m

200.0 °C

1.10E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 1.10E+7 S/m

Unlock all property charts

Specific Electrical conductivity

24 % IACS

Show Material materials with Specific Electrical conductivity of 24 % IACS

spezifischer Widerstand

20.0 °C

7.1E-8 Ω·m

Show Material materials with spezifischer Widerstand of 7.1E-8 Ω·m

200.0 °C

9.1E-8 Ω·m

Show Material materials with spezifischer Widerstand of 9.1E-8 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Blei

1.6 - 2.5 %

Show Material materials with Blei of 1.6 - 2.5 %

Eisen

0.2 - 0.3 %

Show Material materials with Eisen of 0.2 - 0.3 %

Kupfer

59 - 60 %

Show Material materials with Kupfer of 59 - 60 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Zinn

0.3 %

Show Material materials with Zinn of 0.3 %