Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 20.0 °C | 135 GPa Show Material materials with Elastizitätsmodul of 135 GPa | |
Elongation A100 | 20.0 °C | 5 - 8 % Show Material materials with Elongation A100 of 5 - 8 % | |
Elongation A11.3 | 20.0 °C | 10 % Show Material materials with Elongation A11.3 of 10 % | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze Rp 0,2 | 20.0 °C | 260 MPa Show Material materials with Streckgrenze Rp 0,2 of 260 MPa | |
Zugfestigkeit | 20.0 °C | 350 MPa Show Material materials with Zugfestigkeit of 350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.7E-5 - 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 1.8E-5 1/K | |
Schmelzpunkt | 965 - 1100 °C Show Material materials with Schmelzpunkt of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Spezifische Wärmekapazität | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Wärmeleitfähigkeit | 20.0 °C | 167 - 330 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 167 - 330 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 2.60E+7 - 5.40E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 2.60E+7 - 5.40E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Property | Value |
---|---|
Zirkonium | 0.1 - 0.2 % Show Material materials with Zirkonium of 0.1 - 0.2 % |