Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 - 8.41 g/cm³ Show Material materials with Dichte of 8.4 - 8.41 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 22 % Show Material materials with Dehnung of 22 % | |
Elastizitätsmodul | 20.0 °C | 108 GPa Show Material materials with Elastizitätsmodul of 108 GPa | |
Elongation A10 | 20.0 °C | 18 % Show Material materials with Elongation A10 of 18 % | |
Elongation A11.3 | 20.0 °C | 18 % Show Material materials with Elongation A11.3 of 18 % | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 240 - 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 240 - 250 MPa | |
Zugfestigkeit | 20.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.92E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.92E-5 1/K | |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 20.0 °C | 394 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 394 J/(kg·K) | |
100.0 °C | 403 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 403 J/(kg·K) | ||
200.0 °C | 415 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 415 J/(kg·K) | ||
Wärmeleitfähigkeit | 20.0 °C | 71 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 71 W/(m·K) | |
100.0 °C | 79 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 79 W/(m·K) | ||
200.0 °C | 86 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 86 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 8.90E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 8.90E+6 S/m |
Specific Electrical conductivity | 15 % IACS Show Material materials with Specific Electrical conductivity of 15 % IACS |
Chemical properties
Property | Value |
---|---|
Blei | 0.8 % Show Material materials with Blei of 0.8 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Kupfer | 66 - 70 % Show Material materials with Kupfer of 66 - 70 % |
Nickel | 0.5 % Show Material materials with Nickel of 0.5 % |
Silizium | 0.7 - 1.3 % Show Material materials with Silizium of 0.7 - 1.3 % |