Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.28 - 8.3 g/cm³ Show Material materials with Dichte of 8.28 - 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 93 GPa Show Material materials with Elastizitätsmodul of 93 GPa | |
Härte, Brinell | 20.0 °C | 150 [-] Show Material materials with Härte, Brinell of 150 [-] | |
Härte, Vickers | 20.0 °C | 160 [-] Show Material materials with Härte, Vickers of 160 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 20.0 °C | 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 50 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.90E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.90E+6 S/m |
Specific Electrical conductivity | 10 % IACS Show Material materials with Specific Electrical conductivity of 10 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.5 % Show Material materials with Aluminium of 0.3 - 1.5 % |
Blei | 0.8 % Show Material materials with Blei of 0.8 % |
Eisen | 0.5 % Show Material materials with Eisen of 0.5 % |
Kupfer | 58 - 61 % Show Material materials with Kupfer of 58 - 61 % |
Mangan | 1.5 - 2.5 % Show Material materials with Mangan of 1.5 - 2.5 % |
Nickel | 2 - 3 % Show Material materials with Nickel of 2 - 3 % |
Silizium | 0.1 % Show Material materials with Silizium of 0.1 % |
Zinn | 0.5 % Show Material materials with Zinn of 0.5 % |