Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.35 - 8.4 g/cm³ Show Material materials with Dichte of 8.35 - 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 15 - 20 % Show Material materials with Dehnung of 15 - 20 % |
Elastizitätsmodul | 20.0 °C | 112 GPa Show Material materials with Elastizitätsmodul of 112 GPa |
Elongation A10 | 20.0 °C | 16 % Show Material materials with Elongation A10 of 16 % |
Elongation A100 | 20.0 °C | 8 % Show Material materials with Elongation A100 of 8 % |
Elongation A11.3 | 20.0 °C | 10 % Show Material materials with Elongation A11.3 of 10 % |
Härte, Vickers | 20.0 °C | 110 [-] Show Material materials with Härte, Vickers of 110 [-] |
Schubmodule | 20.0 °C | 42 GPa Show Material materials with Schubmodule of 42 GPa |
Streckgrenze Rp 0,2 | 20.0 °C | 180 - 210 MPa Show Material materials with Streckgrenze Rp 0,2 of 180 - 210 MPa |
100.0 °C | 200 MPa Show Material materials with Streckgrenze Rp 0,2 of 200 MPa | |
150.0 °C | 190 MPa Show Material materials with Streckgrenze Rp 0,2 of 190 MPa | |
200.0 °C | 180 MPa Show Material materials with Streckgrenze Rp 0,2 of 180 MPa | |
Zugfestigkeit | 20.0 °C | 400 MPa Show Material materials with Zugfestigkeit of 400 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 20.0 °C | 117 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 117 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.51E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.51E+7 S/m |
spezifischer Widerstand | 20.0 °C | 6.6E-8 Ω·m Show Material materials with spezifischer Widerstand of 6.6E-8 Ω·m |
Chemical properties