Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.24 - 8.3 g/cm³ Show Material materials with Dichte of 8.24 - 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20.0 °C | 93 GPa Show Material materials with Elastizitätsmodul of 93 GPa |
Härte, Brinell | 20.0 °C | 120 - 150 [-] Show Material materials with Härte, Brinell of 120 - 150 [-] |
Härte, Vickers | 20.0 °C | 125 - 155 [-] Show Material materials with Härte, Vickers of 125 - 155 [-] |
Thermisch
Property | Temperature | Value |
---|---|---|
Wärmeleitfähigkeit | 20.0 °C | 63 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 63 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 7.80E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 7.80E+6 S/m |
Specific Electrical conductivity | 13 % IACS Show Material materials with Specific Electrical conductivity of 13 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.3 - 1.3 % Show Material materials with Aluminium of 0.3 - 1.3 % |
Blei | 1 % Show Material materials with Blei of 1 % |
Eisen | 1 % Show Material materials with Eisen of 1 % |
Kupfer | 59 - 61.5 % Show Material materials with Kupfer of 59 - 61.5 % |
Mangan | 0.6 - 1.8 % Show Material materials with Mangan of 0.6 - 1.8 % |
Nickel | 0.6 % Show Material materials with Nickel of 0.6 % |
Silizium | 0.5 % Show Material materials with Silizium of 0.5 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |