Dichte: 8.24 - 8.3 g/cm³

Quick Comparison

Wrought Copper High Copper Alloy

ASTM B196 Grade C17200 TB00

Wrought Copper High Copper Alloy

ASTM B194 Grade C17200 TD04

Wrought Copper High Copper Alloy

EN 1652 Grade C17200 TF00

Nickel Chromium Iron Alloy

VDM® Alloy 718

Geliefert von:

VDM Metals

Wrought Copper High Copper Alloy

ASTM B643 Grade C17200 TH04

Wrought Copper High Copper Alloy

AMPCOLOY® 83 Rolled material

Geliefert von:

AMPCO METAL

Nickel-Eisen-Legierung

Alloy 52 Bar

Nickel-Eisen-Legierung

Alloy 52 Strip/Coil

Unclassified Cobalt Alloy

UGI® PHYNOX® Drawn

Geliefert von:

Ugitech

Nickel-Eisen-Legierung

Alloy 52 Plate

Wrought Copper Brass Yellow Brass

EnviB10 - CuZn40 - ASTM B36 M

Geliefert von:

Lebronze Alloys

Wrought Copper High Copper Alloy

AMPCOLOY® 83 Extrusions

Geliefert von:

AMPCO METAL

Wrought Copper High Copper Alloy

AMPCOLOY® 83 Forgings

Geliefert von:

AMPCO METAL

Wrought Copper High Copper Alloy

AMPCOLOY® 83 Sand castings

Geliefert von:

AMPCO METAL

Wrought Copper High Copper Alloy

C99® O - CuPb1P - C18700

Geliefert von:

Lebronze Alloys

Wrought Copper High Copper Alloy

C99® H12 - CuPb1P - C18700

Geliefert von:

Lebronze Alloys

Wrought Copper High Copper Alloy

C99® H14 - CuPb1P - C18700

Geliefert von:

Lebronze Alloys

Wrought Copper High Copper Alloy

EN 1652 Grade CuBe2 TH