Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.6 g/cm³ Show Material materials with Dichte of 7.6 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 20.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Härte, Brinell | 20.0 °C | 200 [-] Show Material materials with Härte, Brinell of 200 [-] | |
Härte, Vickers | 20.0 °C | 210 [-] Show Material materials with Härte, Vickers of 210 [-] | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Schubmodule | 20.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 20.0 °C | 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 420 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 50 - 57 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 50 - 57 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 4.00E+6 - 7.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 4.00E+6 - 7.00E+6 S/m |
Specific Electrical conductivity | 10.3 % IACS Show Material materials with Specific Electrical conductivity of 10.3 % IACS |
Chemical properties
Property | Value |
---|---|
Aluminium | 8.5 - 11 % Show Material materials with Aluminium of 8.5 - 11 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 3 - 5 % Show Material materials with Eisen of 3 - 5 % |
Kupfer | 76.05 % Show Material materials with Kupfer of 76.05 % |
Mangan | 1 % Show Material materials with Mangan of 1 % |
Nickel | 4 - 6 % Show Material materials with Nickel of 4 - 6 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.4 % Show Material materials with Zink of 0.4 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |