Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 7.4 g/cm³ Show Material materials with Dichte of 7.4 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 3 % Show Material materials with Dehnung of 3 % | |
Elastizitätsmodul | 20.0 °C | 127 GPa Show Material materials with Elastizitätsmodul of 127 GPa | |
Elongation A11.3 | 20.0 °C | 2 % Show Material materials with Elongation A11.3 of 2 % | |
Poissonzahl | 23.0 °C | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Leaded Phosphor Bronze |
Schubmodule | 20.0 °C | 45 GPa Show Material materials with Schubmodule of 45 GPa | |
Streckgrenze Rp 0,2 | 20.0 °C | 550 - 680 MPa Show Material materials with Streckgrenze Rp 0,2 of 550 - 680 MPa | |
Zugfestigkeit | 20.0 °C | 830 MPa Show Material materials with Zugfestigkeit of 830 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.5E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.5E-5 - 1.9E-5 1/K | Typical for Leaded Phosphor Bronze |
Spezifische Wärmekapazität | 23.0 °C | 380 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K) | Typical for Leaded Phosphor Bronze |
Wärmeleitfähigkeit | 20.0 °C | 40 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 40 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.00E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 5.00E+6 S/m |
Chemical properties
Property | Value |
---|---|
Aluminium | 10.5 - 12.5 % Show Material materials with Aluminium of 10.5 - 12.5 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 5 - 7 % Show Material materials with Eisen of 5 - 7 % |
Kupfer | 70.95 % Show Material materials with Kupfer of 70.95 % |
Mangan | 1.5 % Show Material materials with Mangan of 1.5 % |
Nickel | 5 - 7 % Show Material materials with Nickel of 5 - 7 % |
Silizium | 0.2 % Show Material materials with Silizium of 0.2 % |
Zink | 0.5 % Show Material materials with Zink of 0.5 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |