Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.8 - 8.9 g/cm³ Show Material materials with Dichte of 8.8 - 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 7 - 12 % Show Material materials with Dehnung of 7 - 12 % | |
Elastizitätsmodul | 20.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Elongation A10 | 20.0 °C | 5 - 7 % Show Material materials with Elongation A10 of 5 - 7 % | |
Elongation A100 | 20.0 °C | 2 - 3 % Show Material materials with Elongation A100 of 2 - 3 % | |
Elongation A11.3 | 20.0 °C | 4 - 5 % Show Material materials with Elongation A11.3 of 4 - 5 % | |
Härte, Brinell | 20.0 °C | 80 - 110 [-] Show Material materials with Härte, Brinell of 80 - 110 [-] | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze Rp 0,2 | 20.0 °C | 180 - 200 MPa Show Material materials with Streckgrenze Rp 0,2 of 180 - 200 MPa | |
Zugfestigkeit | 20.0 °C | 250 - 350 MPa Show Material materials with Zugfestigkeit of 250 - 350 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 300.0 °C | 1.8E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.8E-5 1/K | |
Schmelzpunkt | 965 - 1100 °C Show Material materials with Schmelzpunkt of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Spezifische Wärmekapazität | 23.0 °C | 377 - 420 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 - 420 J/(kg·K) | Typical for Wrought Copper Pure / Low Alloyed Copper |
Wärmeleitfähigkeit | 20.0 °C | 368 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 368 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 5.00E+7 - 5.45E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 5.00E+7 - 5.45E+7 S/m |
Specific Electrical conductivity | 86 % IACS Show Material materials with Specific Electrical conductivity of 86 % IACS |
Chemical properties
Property | Value |
---|---|
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |
Tellur | 0.4 - 0.7 % Show Material materials with Tellur of 0.4 - 0.7 % |