Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 20 % Show Material materials with Dehnung of 20 % |
Elongation A10 | 20.0 °C | 16 % Show Material materials with Elongation A10 of 16 % |
Streckgrenze Rp 0,2 | 20.0 °C | 160 MPa Show Material materials with Streckgrenze Rp 0,2 of 160 MPa |
Zugfestigkeit | 20.0 °C | 380 MPa Show Material materials with Zugfestigkeit of 380 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 0.8 - 1.6 % Show Material materials with Blei of 0.8 - 1.6 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 59 - 60 % Show Material materials with Kupfer of 59 - 60 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |