Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 12 - 15 % Show Material materials with Dehnung of 12 - 15 % |
Elongation A10 | 20.0 °C | 12 % Show Material materials with Elongation A10 of 12 % |
Elongation A100 | 20.0 °C | 8 - 10 % Show Material materials with Elongation A100 of 8 - 10 % |
Elongation A11.3 | 20.0 °C | 10 % Show Material materials with Elongation A11.3 of 10 % |
Streckgrenze Rp 0,2 | 20.0 °C | 190 - 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 190 - 250 MPa |
Zugfestigkeit | 20.0 °C | 410 MPa Show Material materials with Zugfestigkeit of 410 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 0.8 - 1.6 % Show Material materials with Blei of 0.8 - 1.6 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 59 - 60 % Show Material materials with Kupfer of 59 - 60 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |