Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 - 8.45 g/cm³ Show Material materials with Dichte of 8.4 - 8.45 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 12 - 15 % Show Material materials with Dehnung of 12 - 15 % | |
Elastizitätsmodul | 20.0 °C | 102 GPa Show Material materials with Elastizitätsmodul of 102 GPa | |
Elongation A10 | 20.0 °C | 12 % Show Material materials with Elongation A10 of 12 % | |
Elongation A100 | 20.0 °C | 8 - 10 % Show Material materials with Elongation A100 of 8 - 10 % | |
Elongation A11.3 | 20.0 °C | 10 % Show Material materials with Elongation A11.3 of 10 % | |
Poissonzahl | 20.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 190 - 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 190 - 250 MPa | |
Zugfestigkeit | 20.0 °C | 410 MPa Show Material materials with Zugfestigkeit of 410 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 2E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2E-5 1/K | |
300.0 °C | 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 1/K | ||
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 20.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 109 - 117 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 109 - 117 W/(m·K) | |
200.0 °C | 134 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 134 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.39E+7 - 1.40E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.39E+7 - 1.40E+7 S/m |
200.0 °C | 1.10E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.10E+7 S/m | |
Specific Electrical conductivity | 24 % IACS Show Material materials with Specific Electrical conductivity of 24 % IACS | |
spezifischer Widerstand | 20.0 °C | 7.1E-8 Ω·m Show Material materials with spezifischer Widerstand of 7.1E-8 Ω·m |
200.0 °C | 9.1E-8 Ω·m Show Material materials with spezifischer Widerstand of 9.1E-8 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 1.6 - 2.5 % Show Material materials with Blei of 1.6 - 2.5 % |
Eisen | 0.2 - 0.3 % Show Material materials with Eisen of 0.2 - 0.3 % |
Kupfer | 59 - 60 % Show Material materials with Kupfer of 59 - 60 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |