Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.1 - 8.3 g/cm³ Show Material materials with Dichte of 8.1 - 8.3 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Dehnung | 20.0 °C | 18 - 20 % Show Material materials with Dehnung of 18 - 20 % |
Elastizitätsmodul | 20.0 °C | 95 GPa Show Material materials with Elastizitätsmodul of 95 GPa |
Elongation A10 | 20.0 °C | 15 % Show Material materials with Elongation A10 of 15 % |
Elongation A100 | 20.0 °C | 8 - 10 % Show Material materials with Elongation A100 of 8 - 10 % |
Elongation A11.3 | 20.0 °C | 15 % Show Material materials with Elongation A11.3 of 15 % |
Schubmodule | 20.0 °C | 36 GPa Show Material materials with Schubmodule of 36 GPa |
Streckgrenze Rp 0,2 | 20.0 °C | 250 - 300 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 - 300 MPa |
Zugfestigkeit | 20.0 °C | 440 - 540 MPa Show Material materials with Zugfestigkeit of 440 - 540 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.9E-5 1/K | |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 20.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | |
Wärmeleitfähigkeit | 20.0 °C | 67 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 67 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 8.70E+6 S/m Show Material materials with Elektrische Leitfähigkeit of 8.70E+6 S/m |
spezifischer Widerstand | 20.0 °C | 1.15E-7 Ω·m Show Material materials with spezifischer Widerstand of 1.15E-7 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.2 - 0.6 % Show Material materials with Aluminium of 0.2 - 0.6 % |
Blei | 1 - 2 % Show Material materials with Blei of 1 - 2 % |
Eisen | 0.3 - 0.5 % Show Material materials with Eisen of 0.3 - 0.5 % |
Kupfer | 57 - 59 % Show Material materials with Kupfer of 57 - 59 % |
Mangan | 0.4 - 1.8 % Show Material materials with Mangan of 0.4 - 1.8 % |
Nickel | 0.3 - 1 % Show Material materials with Nickel of 0.3 - 1 % |
Silizium | 0.1 - 0.4 % Show Material materials with Silizium of 0.1 - 0.4 % |
Zinn | 0.3 - 0.5 % Show Material materials with Zinn of 0.3 - 0.5 % |