Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Dichte of 8.4 - 8.9 g/cm³ | Typical for Wrought Copper Nickel Silver Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 12 % Show Material materials with Dehnung of 12 % | |
Elastizitätsmodul | 23.0 °C | 120 - 140 GPa Show Material materials with Elastizitätsmodul of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Elongation A10 | 20.0 °C | 10 % Show Material materials with Elongation A10 of 10 % | |
Elongation A100 | 20.0 °C | 8 % Show Material materials with Elongation A100 of 8 % | |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Streckgrenze Rp 0,2 | 20.0 °C | 400 MPa Show Material materials with Streckgrenze Rp 0,2 of 400 MPa | |
Zugfestigkeit | 20.0 °C | 510 MPa Show Material materials with Zugfestigkeit of 510 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Schmelzpunkt | 875 - 1135 °C Show Material materials with Schmelzpunkt of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Blei | 2.3 - 3.3 % Show Material materials with Blei of 2.3 - 3.3 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 47 - 50 % Show Material materials with Kupfer of 47 - 50 % |
Mangan | 1.5 - 3 % Show Material materials with Mangan of 1.5 - 3 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |