Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | -195.0 °C | 108 GPa Show Material materials with Elastizitätsmodul of 108 GPa | |
-100.0 °C | 106 GPa Show Material materials with Elastizitätsmodul of 106 GPa | ||
20.0 °C | 105 GPa Show Material materials with Elastizitätsmodul of 105 GPa | ||
50.0 °C | 100 GPa Show Material materials with Elastizitätsmodul of 100 GPa | ||
100.0 °C | 93 GPa Show Material materials with Elastizitätsmodul of 93 GPa | ||
150.0 °C | 91 GPa Show Material materials with Elastizitätsmodul of 91 GPa | ||
200.0 °C | 89 GPa Show Material materials with Elastizitätsmodul of 89 GPa | ||
250.0 °C | 83 GPa Show Material materials with Elastizitätsmodul of 83 GPa | ||
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.1 % Show Material materials with Aluminium of 0.1 % |
Blei | 1.6 - 2.5 % Show Material materials with Blei of 1.6 - 2.5 % |
Eisen | 0.4 % Show Material materials with Eisen of 0.4 % |
Kupfer | 59 - 60 % Show Material materials with Kupfer of 59 - 60 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 - 0.5 % Show Material materials with Zinn of 0.2 - 0.5 % |