EN 12166 Grade CuNi12Zn24 H200

View suppliers (9)
Want to keep this datasheet? Save it now in your required format

Description

Material CuNi12Zn24, mat. No. CW403J is an alloy of high strength and hardness. To the comparabel DIN-mark CuNi12Zn24, mat. No. 2.0730, acc. to DIN 17663 : 1983-12 applies: Strength is further increasable due to the high strain hardening capability. The material does not embrittle at low temperatures. Low electrical and thermal conductivity. The alloy is non-magnetic, corrosion resistance is better than for pure copper. Processing properties: warm forming: moderately cold forming: very good machinability: moderately hard and soft soldering: very good TIG-welding: very good burnishing: very good Application: In electrical engineering and electronics for springs, contacts, membranes as well as in precision engineering and in equipment manufacturing. In food industry, for musical instruments, glasses frames, safety keys as well as in construction trade for paneling, show-cases and stairrails.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.67 - 8.7 g/cm³

Show Material materials with Dichte of 8.67 - 8.7 g/cm³

Mechanisch

PropertyTemperatureValue

Elastizitätsmodul

20.0 °C

125 GPa

Show Material materials with Elastizitätsmodul of 125 GPa

Härte, Vickers

20.0 °C

200 [-]

Show Material materials with Härte, Vickers of 200 [-]

Poissonzahl

20.0 °C

0.34 [-]

Show Material materials with Poissonzahl of 0.34 [-]

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

300.0 °C

1.65E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.65E-5 1/K

Schmelzpunkt

875 - 1135 °C

Show Material materials with Schmelzpunkt of 875 - 1135 °C

Typical for Wrought Copper Nickel Silver Grade

Spezifische Wärmekapazität

20.0 °C

380 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 380 J/(kg·K)

Wärmeleitfähigkeit

20.0 °C

42 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 42 W/(m·K)

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

4.40E+6 S/m

Show Material materials with Elektrische Leitfähigkeit of 4.40E+6 S/m

Specific Electrical conductivity

8 % IACS

Show Material materials with Specific Electrical conductivity of 8 % IACS

Chemical properties

PropertyValue

Blei

0.03 %

Show Material materials with Blei of 0.03 %

Eisen

0.3 %

Show Material materials with Eisen of 0.3 %

Kupfer

63 - 66 %

Show Material materials with Kupfer of 63 - 66 %

Mangan

0.5 %

Show Material materials with Mangan of 0.5 %

Nickel

11 - 13 %

Show Material materials with Nickel of 11 - 13 %

Zinn

0.03 %

Show Material materials with Zinn of 0.03 %