Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.46 - 8.5 g/cm³ Show Material materials with Dichte of 8.46 - 8.5 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 20.0 °C | 105 - 110 GPa Show Material materials with Elastizitätsmodul of 105 - 110 GPa |
Härte, Brinell | 20.0 °C | 70 - 120 [-] Show Material materials with Härte, Brinell of 70 - 120 [-] |
Härte, Vickers | 20.0 °C | 80 - 130 [-] Show Material materials with Härte, Vickers of 80 - 130 [-] |
Schubmodule | 20.0 °C | 39 GPa Show Material materials with Schubmodule of 39 GPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 200.0 °C | 2.04E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.04E-5 1/K | |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 20.0 °C | 113 - 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 113 - 116 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.47E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.47E+7 S/m |
Specific Electrical conductivity | 25 % IACS Show Material materials with Specific Electrical conductivity of 25 % IACS | |
spezifischer Widerstand | 20.0 °C | 6.8E-8 Ω·m Show Material materials with spezifischer Widerstand of 6.8E-8 Ω·m |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 1.6 - 2.5 % Show Material materials with Blei of 1.6 - 2.5 % |
Eisen | 0.1 % Show Material materials with Eisen of 0.1 % |
Kupfer | 62 - 63.5 % Show Material materials with Kupfer of 62 - 63.5 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.1 % Show Material materials with Zinn of 0.1 % |