Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 - 8.47 g/cm³ Show Material materials with Dichte of 8.4 - 8.47 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | -196.0 °C | 40 % Show Material materials with Dehnung of 40 % | |
-78.0 °C | 34 % Show Material materials with Dehnung of 34 % | ||
20.0 °C | 25 - 33 % Show Material materials with Dehnung of 25 - 33 % | ||
Elastizitätsmodul | 20.0 °C | 96 - 97 GPa Show Material materials with Elastizitätsmodul of 96 - 97 GPa | |
Härte, Brinell | 20.0 °C | 80 - 115 [-] Show Material materials with Härte, Brinell of 80 - 115 [-] | |
Härte, Vickers | 20.0 °C | 85 - 120 [-] Show Material materials with Härte, Vickers of 85 - 120 [-] | |
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa | |
Zugfestigkeit | -196.0 °C | 575 MPa Show Material materials with Zugfestigkeit of 575 MPa | |
-78.0 °C | 460 MPa Show Material materials with Zugfestigkeit of 460 MPa | ||
20.0 °C | 360 - 425 MPa Show Material materials with Zugfestigkeit of 360 - 425 MPa | ||
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 100.0 °C | 1.93E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.93E-5 1/K | |
200.0 °C | 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 1/K | ||
300.0 °C | 2.14E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.14E-5 1/K | ||
800.0 °C | 2.47E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.47E-5 1/K | ||
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 20.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | |
Wärmeleitfähigkeit | -200.0 °C | 50 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 50 W/(m·K) | |
20.0 °C | 113 - 123 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 113 - 123 W/(m·K) | ||
Elektrisch
Property | Temperature | Value |
---|---|---|
Elektrische Leitfähigkeit | 20.0 °C | 1.46E+7 - 1.50E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.46E+7 - 1.50E+7 S/m |
200.0 °C | 1.20E+7 S/m Show Material materials with Elektrische Leitfähigkeit of 1.20E+7 S/m | |
Specific Electrical conductivity | 25 - 25.2 % IACS Show Material materials with Specific Electrical conductivity of 25 - 25.2 % IACS | |
spezifischer Widerstand | 20.0 °C | 6.6E-8 Ω·m Show Material materials with spezifischer Widerstand of 6.6E-8 Ω·m |
200.0 °C | 8.3E-8 Ω·m Show Material materials with spezifischer Widerstand of 8.3E-8 Ω·m | |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 2.5 - 3.5 % Show Material materials with Blei of 2.5 - 3.5 % |
Eisen | 0.3 % Show Material materials with Eisen of 0.3 % |
Kupfer | 57 - 59 % Show Material materials with Kupfer of 57 - 59 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.3 % Show Material materials with Zinn of 0.3 % |