EN 12167 Grade CuZn39Pb3 H110

View suppliers (30)
Want to keep this datasheet? Save it now in your required format

Description

Material CuZn39Pb3, mat. No. CW614N, is an unhardenable wrought alloy. to the comparable make CuZn39Pb3, mat. No. 2.0401 acc. to DIN 17660 : 1983-12 applies: High hardness and strength parameter are achievable by cold forming only. Thermal and electrical conductivity are lower than for unleaded brass of the same Zn-content. Machinability is improved by Pb-addition. Corrosion resistance to water, several saline solutions and organic liquids is also lower than for unleaded alloys of the same zinc-content. Processing properties: warm forming: very good cold forming: unfavorable machinability: very good hard soldering: moderately soft soldering: very good TIG-welding: unfavorable burnishing: very good Application: Main alloy of the brass materials for machining on automats. Use for all types of form turning parts, in precision engineering as well as in watch and electrical industry.

Related Standards

Equivalent Materials

Diese Materialdaten wurden von WIAM zur Verfügung gestellt

Alle Daten beziehen sich auf Raumtemperatur soweit nicht anderweitig spezifiziert. SI Einheiten werden verwendt soweit nicht anderweitig spezifiziert.
Äquivalente Standards sind ähnlich zu einem oder mehreren Standards die der Anbieter angegeben hat. Manche äquivalente Standards können strikter sein oder außerhalb der Bedingungen des ursprünglichen Standards.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Eigenschaften

Allgemein

PropertyTemperatureValue

Dichte

20.0 °C

8.4 - 8.47 g/cm³

Show Material materials with Dichte of 8.4 - 8.47 g/cm³

Mechanisch

PropertyTemperatureValueComment

Elastizitätsmodul

20.0 °C

96 - 97 GPa

Show Material materials with Elastizitätsmodul of 96 - 97 GPa

Härte, Brinell

20.0 °C

110 - 160 [-]

Show Material materials with Härte, Brinell of 110 - 160 [-]

Härte, Vickers

20.0 °C

120 - 170 [-]

Show Material materials with Härte, Vickers of 120 - 170 [-]

Schubmodule

23.0 °C

40 GPa

Show Material materials with Schubmodule of 40 GPa

Typical for Wrought Copper Brass

Streckgrenze Rp 0,2

20.0 °C

250 MPa

Show Material materials with Streckgrenze Rp 0,2 of 250 MPa

Zugfestigkeit

20.0 °C

430 MPa

Show Material materials with Zugfestigkeit of 430 MPa

Thermisch

PropertyTemperatureValueComment

Koeffizient der thermischen Ausdehnung

100.0 °C

1.93E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 1.93E-5 1/K

200.0 °C

2.1E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.1E-5 1/K

300.0 °C

2.14E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.14E-5 1/K

800.0 °C

2.47E-5 1/K

Show Material materials with Koeffizient der thermischen Ausdehnung of 2.47E-5 1/K

Schmelzpunkt

875 - 1075 °C

Show Material materials with Schmelzpunkt of 875 - 1075 °C

Typical for Wrought Copper Brass

Spezifische Wärmekapazität

20.0 °C

377 J/(kg·K)

Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K)

Wärmeleitfähigkeit

-200.0 °C

50 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 50 W/(m·K)

20.0 °C

113 - 123 W/(m·K)

Show Material materials with Wärmeleitfähigkeit of 113 - 123 W/(m·K)

Unlock all property charts

Elektrisch

PropertyTemperatureValue

Elektrische Leitfähigkeit

20.0 °C

1.46E+7 - 1.50E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 1.46E+7 - 1.50E+7 S/m

200.0 °C

1.20E+7 S/m

Show Material materials with Elektrische Leitfähigkeit of 1.20E+7 S/m

Unlock all property charts

Specific Electrical conductivity

25 - 25.2 % IACS

Show Material materials with Specific Electrical conductivity of 25 - 25.2 % IACS

spezifischer Widerstand

20.0 °C

6.6E-8 Ω·m

Show Material materials with spezifischer Widerstand of 6.6E-8 Ω·m

200.0 °C

8.3E-8 Ω·m

Show Material materials with spezifischer Widerstand of 8.3E-8 Ω·m

Unlock all property charts

Chemical properties

PropertyValue

Aluminium

0.05 %

Show Material materials with Aluminium of 0.05 %

Blei

2.5 - 3.5 %

Show Material materials with Blei of 2.5 - 3.5 %

Eisen

0.3 %

Show Material materials with Eisen of 0.3 %

Kupfer

57 - 59 %

Show Material materials with Kupfer of 57 - 59 %

Nickel

0.3 %

Show Material materials with Nickel of 0.3 %

Zinn

0.3 %

Show Material materials with Zinn of 0.3 %