Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 55 % Show Material materials with Dehnung of 55 % | |
Elastizitätsmodul | 20.0 °C | 110 GPa Show Material materials with Elastizitätsmodul of 110 GPa | |
50.0 °C | 110 GPa Show Material materials with Elastizitätsmodul of 110 GPa | ||
100.0 °C | 108 GPa Show Material materials with Elastizitätsmodul of 108 GPa | ||
150.0 °C | 107 GPa Show Material materials with Elastizitätsmodul of 107 GPa | ||
200.0 °C | 106 GPa Show Material materials with Elastizitätsmodul of 106 GPa | ||
250.0 °C | 105 GPa Show Material materials with Elastizitätsmodul of 105 GPa | ||
Schubmodule | 23.0 °C | 40 GPa Show Material materials with Schubmodule of 40 GPa | Typical for Wrought Copper Brass |
Streckgrenze Rp 0,2 | 20.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 0,2 of 120 MPa | |
Streckgrenze Rp 1,0 | 20.0 °C | 130 MPa Show Material materials with Streckgrenze Rp 1,0 of 130 MPa | |
50.0 °C | 130 MPa Show Material materials with Streckgrenze Rp 1,0 of 130 MPa | ||
100.0 °C | 125 MPa Show Material materials with Streckgrenze Rp 1,0 of 125 MPa | ||
150.0 °C | 125 MPa Show Material materials with Streckgrenze Rp 1,0 of 125 MPa | ||
200.0 °C | 120 MPa Show Material materials with Streckgrenze Rp 1,0 of 120 MPa | ||
Zugfestigkeit | 20.0 °C | 340 MPa Show Material materials with Zugfestigkeit of 340 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 - 2.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 - 2.1E-5 1/K | Typical for Wrought Copper Brass |
Schmelzpunkt | 875 - 1075 °C Show Material materials with Schmelzpunkt of 875 - 1075 °C | Typical for Wrought Copper Brass | |
Spezifische Wärmekapazität | 23.0 °C | 371 - 418 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 371 - 418 J/(kg·K) | Typical for Wrought Copper Brass |
Wärmeleitfähigkeit | 23.0 °C | 100 - 234 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 100 - 234 W/(m·K) | Typical for Wrought Copper Brass |
Chemical properties
Property | Value |
---|---|
Aluminium | 1.8 - 2.3 % Show Material materials with Aluminium of 1.8 - 2.3 % |
Arsen | 0.02 - 0.06 % Show Material materials with Arsen of 0.02 - 0.06 % |
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.07 % Show Material materials with Eisen of 0.07 % |
Kupfer | 76 - 79 % Show Material materials with Kupfer of 76 - 79 % |
Mangan | 0.1 % Show Material materials with Mangan of 0.1 % |
Nickel | 0.1 % Show Material materials with Nickel of 0.1 % |
Phosphor | 0.01 % Show Material materials with Phosphor of 0.01 % |