Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 20.0 °C | 8.4 g/cm³ Show Material materials with Dichte of 8.4 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Brinell | 20.0 °C | 110 - 160 [-] Show Material materials with Härte, Brinell of 110 - 160 [-] |
Härte, Vickers | 20.0 °C | 120 - 170 [-] Show Material materials with Härte, Vickers of 120 - 170 [-] |
Streckgrenze Rp 0,2 | 20.0 °C | 250 MPa Show Material materials with Streckgrenze Rp 0,2 of 250 MPa |
Zugfestigkeit | 20.0 °C | 410 MPa Show Material materials with Zugfestigkeit of 410 MPa |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 % Show Material materials with Aluminium of 0.05 % |
Blei | 0.8 - 1.6 % Show Material materials with Blei of 0.8 - 1.6 % |
Eisen | 0.2 % Show Material materials with Eisen of 0.2 % |
Kupfer | 59 - 60 % Show Material materials with Kupfer of 59 - 60 % |
Nickel | 0.3 % Show Material materials with Nickel of 0.3 % |
Zinn | 0.2 % Show Material materials with Zinn of 0.2 % |