Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 23.0 °C | 8.4 - 8.9 g/cm³ Show Material materials with Dichte of 8.4 - 8.9 g/cm³ | Typical for Wrought Copper Nickel Silver Grade |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 - 140 GPa Show Material materials with Elastizitätsmodul of 120 - 140 GPa | Typical for Wrought Copper Nickel Silver Grade |
Hardness, Rockwell Superficial 30-T | 23.0 °C | 80 [-] Show Material materials with Hardness, Rockwell Superficial 30-T of 80 [-] | |
Härte, Rockwell B | 23.0 °C | 97 - 100 [-] Show Material materials with Härte, Rockwell B of 97 - 100 [-] | |
Poissonzahl | 23.0 °C | 0.32 [-] Show Material materials with Poissonzahl of 0.32 [-] | Typical for Wrought Copper Nickel Silver Grade |
Zugfestigkeit | 23.0 °C | 745 - 850 MPa Show Material materials with Zugfestigkeit of 745 - 850 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.9E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.9E-5 1/K | Typical for Wrought Copper Nickel Silver Grade |
Schmelzpunkt | 875 - 1135 °C Show Material materials with Schmelzpunkt of 875 - 1135 °C | Typical for Wrought Copper Nickel Silver Grade | |
Spezifische Wärmekapazität | 23.0 °C | 377 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 377 J/(kg·K) | Typical for Wrought Copper Nickel Silver Grade |
Wärmeleitfähigkeit | 23.0 °C | 21 - 116 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 21 - 116 W/(m·K) | Typical for Wrought Copper Nickel Silver Grade |
Chemical properties
Property | Value |
---|---|
Blei | 0.05 % Show Material materials with Blei of 0.05 % |
Eisen | 0.25 % Show Material materials with Eisen of 0.25 % |
Kupfer | 53.5 - 56.5 % Show Material materials with Kupfer of 53.5 - 56.5 % |
Mangan | 0.5 % Show Material materials with Mangan of 0.5 % |
Nickel | 16.5 - 19.5 % Show Material materials with Nickel of 16.5 - 19.5 % |