Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 35 % Show Material materials with Dehnung of 35 % | |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze | 23.0 °C | 85 MPa Show Material materials with Streckgrenze of 85 MPa | |
Zugfestigkeit | 23.0 °C | 240 MPa Show Material materials with Zugfestigkeit of 240 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.7E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.7E-5 1/K |
Schmelzpunkt | 1050 °C Show Material materials with Schmelzpunkt of 1050 °C | |
Spezifische Wärmekapazität | 23.0 °C | 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 390 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 360 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 360 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Kupfer | 99.2 - 99.6 % Show Material materials with Kupfer of 99.2 - 99.6 % |
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |
Tellur | 0.4 - 0.7 % Show Material materials with Tellur of 0.4 - 0.7 % |