Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8 g/cm³ Show Material materials with Dichte of 8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 40 % Show Material materials with Dehnung of 40 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Austenitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Austenitic Stainless Steel |
Streckgrenze | 23.0 °C | 310 MPa Show Material materials with Streckgrenze of 310 MPa | |
Zugfestigkeit | 23.0 °C | 680 MPa Show Material materials with Zugfestigkeit of 680 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | |
Schmelzpunkt | 1230 - 1480 °C Show Material materials with Schmelzpunkt of 1230 - 1480 °C | Typical for Austenitic Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 14 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 14 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 8.5E-7 Ω·m Show Material materials with spezifischer Widerstand of 8.5E-7 Ω·m | Typical for Austenitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 16.5 - 20 % Show Material materials with Chrom of 16.5 - 20 % |
Eisen | 54.4 - 66.9 % Show Material materials with Eisen of 54.4 - 66.9 % |
Kohlenstoff | 0 - 0.03 % Show Material materials with Kohlenstoff of 0 - 0.03 % |
Mangan | 0 - 2 % Show Material materials with Mangan of 0 - 2 % |
Molybdän | 4 - 5 % Show Material materials with Molybdän of 4 - 5 % |
Nickel | 12.5 - 17.5 % Show Material materials with Nickel of 12.5 - 17.5 % |
Phosphor | 0 - 0.05 % Show Material materials with Phosphor of 0 - 0.05 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |
Stickstoff | 0.1 - 0.22 % Show Material materials with Stickstoff of 0.1 - 0.22 % |