Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.9 g/cm³ Show Material materials with Dichte of 7.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 17 % Show Material materials with Dehnung of 17 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Duplex Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Duplex Stainless Steel |
Streckgrenze | 23.0 °C | 610 MPa Show Material materials with Streckgrenze of 610 MPa | |
Zugfestigkeit | 23.0 °C | 870 MPa Show Material materials with Zugfestigkeit of 870 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.1E-5 1/K | |
Max. Betriebstemperatur | 300 °C Show Material materials with Max. Betriebstemperatur of 300 °C | Typical for Duplex Stainless Steel | |
Schmelzpunkt | 1375 - 1450 °C Show Material materials with Schmelzpunkt of 1375 - 1450 °C | Typical for Duplex Stainless Steel | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 15 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 15 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 24 - 26 % Show Material materials with Chrom of 24 - 26 % |
Eisen | 58.1 - 66.8 % Show Material materials with Eisen of 58.1 - 66.8 % |
Kohlenstoff | 0 - 0.03 % Show Material materials with Kohlenstoff of 0 - 0.03 % |
Kupfer | 0 - 0.5 % Show Material materials with Kupfer of 0 - 0.5 % |
Mangan | 0 - 2 % Show Material materials with Mangan of 0 - 2 % |
Molybdän | 3 - 5 % Show Material materials with Molybdän of 3 - 5 % |
Nickel | 6 - 8 % Show Material materials with Nickel of 6 - 8 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.02 % Show Material materials with Schwefel of 0 - 0.02 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |
Stickstoff | 0.24 - 0.35 % Show Material materials with Stickstoff of 0.24 - 0.35 % |