Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.83 - 8.9 g/cm³ Show Material materials with Dichte of 8.83 - 8.9 g/cm³ |
Abmessung
Property | Value | Comment | |
---|---|---|---|
Außendurchmesser | 0.76 - 406 mm Show Material materials with Außendurchmesser of 0.76 - 406 mm | Rod | |
Breite | 1.27 - 559 mm Show Material materials with Breite of 1.27 - 559 mm | ||
Dicke | 0.05 - 254 mm Show Material materials with Dicke of 0.05 - 254 mm | Bar | |
Durchmesser | 1.27 - 12.7 mm Show Material materials with Durchmesser of 1.27 - 12.7 mm | ||
Länge | 610 - 91000 mm Show Material materials with Länge of 610 - 91000 mm | max. Rod and Bar | |
Wall thickness | Typically 10 to 20% of OD |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefähigkeit 90°, in longitudinaler Richtung | 23.0 °C | 1 [-] Show Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 1 [-] | for strip with 0.25mm and thinner. |
Biegefähigkeit 90°, in transversaler Richtung | 23.0 °C | 2 [-] Show Material materials with Biegefähigkeit 90°, in transversaler Richtung of 2 [-] | for strip with 0.25mm and thinner. |
Dehnung | 23.0 °C | 8 - 25 % Show Material materials with Dehnung of 8 - 25 % | for strip with 0.1mm and thicker.,min. |
Elastizitätsmodul | 23.0 °C | 120 - 138 GPa Show Material materials with Elastizitätsmodul of 120 - 138 GPa | |
Härte, Rockwell B | 23.0 °C | 92 - 100 [-] Show Material materials with Härte, Rockwell B of 92 - 100 [-] | |
Härte, Vickers | 23.0 °C | 195 - 275 [-] Show Material materials with Härte, Vickers of 195 - 275 [-] | |
Streckgrenze Rp 0,2 | 23.0 °C | 550 - 760 MPa Show Material materials with Streckgrenze Rp 0,2 of 550 - 760 MPa | |
Zugfestigkeit | 23.0 °C | 680 - 900 MPa Show Material materials with Zugfestigkeit of 680 - 900 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 - 1.76E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 - 1.76E-5 1/K |
Schmelzpunkt | 1030 - 1040 °C Show Material materials with Schmelzpunkt of 1030 - 1040 °C | |
Spezifische Wärmekapazität | 23.0 °C | 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 390 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 210 - 240 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 210 - 240 W/(m·K) |
Elektrisch
Property | Temperature | Value |
---|---|---|
Specific Electrical conductivity | 45 - 60 % IACS Show Material materials with Specific Electrical conductivity of 45 - 60 % IACS | |
spezifischer Widerstand | 23.0 °C | 2.9E-6 - 3.8E-6 Ω·m Show Material materials with spezifischer Widerstand of 2.9E-6 - 3.8E-6 Ω·m |
Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 0 - 0.2 % Show Material materials with Aluminium of 0 - 0.2 % | |
Andere | 0 - 0.5 % Show Material materials with Andere of 0 - 0.5 % | |
Beryllium | 0.2 - 0.6 % Show Material materials with Beryllium of 0.2 - 0.6 % | |
Eisen | 0 - 0.1 % Show Material materials with Eisen of 0 - 0.1 % | |
Kobalt | 0 - 0.3 % Show Material materials with Kobalt of 0 - 0.3 % | |
Kupfer | 95.9 - 98.4 % Show Material materials with Kupfer of 95.9 - 98.4 % | Balance |
Nickel | 1.4 - 2.2 % Show Material materials with Nickel of 1.4 - 2.2 % | |
Silizium | 0 - 0.2 % Show Material materials with Silizium of 0 - 0.2 % |
Technological properties
Property | ||
---|---|---|
Application areas | Typical applications include high reliability spring contacts for switches and relays.,Typical applications for parts finished by forging or extrusion of these alloys include continuous casting mold components and resistance welding components.,Typical applications include resistance welding components, and inserts for metal die casting, injection molding and blow molding.,Typical applications include dies casting plunger tips and dies for steel extrusion.,Typical applications include heat exchanger tubing and resistance welding components.,Typical applications include coil springs and formed wire contacts. |