Allgemein
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Dichte | 2.81 g/cm³ Show Material materials with Dichte of 2.81 g/cm³ | T73511 | BS L160 | Bar |
3.1 g/cm³ Show Material materials with Dichte of 3.1 g/cm³ | T73511 |
Mechanisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Dehnung | 6.0 % Show Material materials with Dehnung of 6.0 % | T73511 | AA Standards, ASTM B221 | A100 | |
7.0 % Show Material materials with Dehnung of 7.0 % | T73511 | AA Standards, ASTM B221 | A100 | ||
7.0 % Show Material materials with Dehnung of 7.0 % | T73511 | AA Standards, ASTM B221 | A50 | ||
7.0 - 8.0 % Show Material materials with Dehnung of 7.0 - 8.0 % | T73511 | BS L160 | Bar | ||
8.0 % Show Material materials with Dehnung of 8.0 % | T73511 | AA Standards, ASTM B221 | A50 | ||
8.1 % Show Material materials with Dehnung of 8.1 % | T73511 | ||||
Elastizitätsmodul | 72.0 GPa Show Material materials with Elastizitätsmodul of 72.0 GPa | T73511 | BS L160 | Bar | |
Plane-Strain Fracture Toughnes | 22.0 - 35.0 MPa·√m Show Material materials with Plane-Strain Fracture Toughnes of 22.0 - 35.0 MPa·√m | Typical for Wrought 7000 Series Aluminium | |||
Poissonzahl | 0.33 [-] Show Material materials with Poissonzahl of 0.33 [-] | Typical for Wrought 7000 Series Aluminium | |||
Schubmodule | 26.4 - 27.1 GPa Show Material materials with Schubmodule of 26.4 - 27.1 GPa | Typical for Wrought 7000 Series Aluminium | |||
Streckgrenze | 365.0 - 420.0 MPa Show Material materials with Streckgrenze of 365.0 - 420.0 MPa | T73511 | BS L160 | Bar | RP02 |
380.0 MPa Show Material materials with Streckgrenze of 380.0 MPa | T73511 | AA Standards, ASTM B221 | RP02 | ||
395.0 MPa Show Material materials with Streckgrenze of 395.0 MPa | T73511 | AA Standards, ASTM B221 | RP02 | ||
400.0 MPa Show Material materials with Streckgrenze of 400.0 MPa | T73511 | AA Standards, ASTM B221 | RP02 | ||
405.0 MPa Show Material materials with Streckgrenze of 405.0 MPa | T73511 | AA Standards, ASTM B221 | RP02 | ||
420.0 MPa Show Material materials with Streckgrenze of 420.0 MPa | T73511 | AA Standards, ASTM B221 | RP02 | ||
430.0 MPa Show Material materials with Streckgrenze of 430.0 MPa | T73511 | ||||
Zugfestigkeit | 425.0 - 485.0 MPa Show Material materials with Zugfestigkeit of 425.0 - 485.0 MPa | T73511 | BS L160 | Bar | |
450.0 MPa Show Material materials with Zugfestigkeit of 450.0 MPa | T73511 | AA Standards, ASTM B221 | |||
470.0 MPa Show Material materials with Zugfestigkeit of 470.0 MPa | T73511 | AA Standards, ASTM B221 | |||
475.0 MPa Show Material materials with Zugfestigkeit of 475.0 MPa | T73511 | AA Standards, ASTM B221 | |||
485.0 MPa Show Material materials with Zugfestigkeit of 485.0 MPa | T73511 | AA Standards, ASTM B221 | |||
510.0 MPa Show Material materials with Zugfestigkeit of 510.0 MPa | T73511 |
Thermisch
Property | Value | Condition | Related Standards | Shape |
---|---|---|---|---|
Koeffizient der thermischen Ausdehnung | 2.3e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.3e-05 1/K | T73511 | ||
2.35e-05 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 2.35e-05 1/K | T73511 | BS L160 | Bar | |
Schmelzpunkt | 480.0 °C Show Material materials with Schmelzpunkt of 480.0 °C | T73511 | ||
635.0 °C Show Material materials with Schmelzpunkt of 635.0 °C | T73511 | BS L160 | Bar | |
Spezifische Wärmekapazität | 910.0 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 910.0 J/(kg·K) | T73511 | ||
Wärmeleitfähigkeit | 130.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 130.0 W/(m·K) | T73511 | ||
134.0 - 160.0 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 134.0 - 160.0 W/(m·K) | T73511 | BS L160 | Bar |
Elektrisch
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Elektrische Leitfähigkeit | 18000000.0 - 34000000.0 S/m Show Material materials with Elektrische Leitfähigkeit of 18000000.0 - 34000000.0 S/m | Typical for Wrought 7000 Series Aluminium | |||
spezifischer Widerstand | 4.31e-08 Ω·m Show Material materials with spezifischer Widerstand of 4.31e-08 Ω·m | T73511 | BS L160 | Bar |
Chemical properties
Property | Value | Condition | Related Standards | Shape | Comment |
---|---|---|---|---|---|
Aluminium | 86.9 - 91.4 % Show Material materials with Aluminium of 86.9 - 91.4 % | T73511 | |||
Andere | 0.15 % Show Material materials with Andere of 0.15 % | T73511 | BS L160 | Bar | Total |
Chrom | 0.18 - 0.28 % Show Material materials with Chrom of 0.18 - 0.28 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Eisen | 0.50 % Show Material materials with Eisen of 0.50 % | T73511 | AA Standards, ASTM B221 | ||
0.5 % Show Material materials with Eisen of 0.5 % | T73511 | BS L160 | Bar | ||
Kupfer | 1.2 - 2.0 % Show Material materials with Kupfer of 1.2 - 2.0 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Magnesium | 2.1 - 2.9 % Show Material materials with Magnesium of 2.1 - 2.9 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Mangan | 0.3 % Show Material materials with Mangan of 0.3 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Silizium | 0.4 % Show Material materials with Silizium of 0.4 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Titan | 0.2 % Show Material materials with Titan of 0.2 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Zink | 5.1 - 6.1 % Show Material materials with Zink of 5.1 - 6.1 % | T73511 | AA Standards, ASTM B221, BS L160 | Bar | |
Zirkonium | 0.25 % Show Material materials with Zirkonium of 0.25 % | T73511 | BS L160 | Bar | Ti + Zr |
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace | |
Brazing | general: no brazing is known or developed | |
Corrosion properties | Stress corrosion cracking: Operational damage in areas with tensile stresses transverse to the grain structure, limited damage to laboratory samples, general: good, without protection in industrial or seawater atmosphere | |
General machinability | General: poor (O), good to acceptable | |
Workability | general (condition): not suitable |