Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.2 g/cm³ Show Material materials with Dichte of 8.2 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 9 % Show Material materials with Dehnung of 9 % | |
Elastizitätsmodul | 23.0 °C | 190 GPa Show Material materials with Elastizitätsmodul of 190 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Maraging Steel |
Streckgrenze | 23.0 °C | 2100 MPa Show Material materials with Streckgrenze of 2100 MPa | |
Zugfestigkeit | 23.0 °C | 2030 MPa Show Material materials with Zugfestigkeit of 2030 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K | |
Schmelzpunkt | 1425 - 1505 °C Show Material materials with Schmelzpunkt of 1425 - 1505 °C | Typical for Maraging Steel | |
Spezifische Wärmekapazität | 23.0 °C | 440 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 440 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 20 - 25 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 20 - 25 W/(m·K) | Typical for Maraging Steel |
Chemical properties
Property | Value |
---|---|
Aluminium | 0.05 - 0.15 % Show Material materials with Aluminium of 0.05 - 0.15 % |
Bor | 0 - 3E-3 % Show Material materials with Bor of 0 - 3E-3 % |
Eisen | 65 - 68.4 % Show Material materials with Eisen of 65 - 68.4 % |
Kalzium | 0 - 0.05 % Show Material materials with Kalzium of 0 - 0.05 % |
Kobalt | 8.5 - 9.5 % Show Material materials with Kobalt of 8.5 - 9.5 % |
Kohlenstoff | 0 - 0.03 % Show Material materials with Kohlenstoff of 0 - 0.03 % |
Mangan | 0 - 0.1 % Show Material materials with Mangan of 0 - 0.1 % |
Molybdän | 4.6 - 5.2 % Show Material materials with Molybdän of 4.6 - 5.2 % |
Nickel | 18 - 19 % Show Material materials with Nickel of 18 - 19 % |
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |
Schwefel | 0 - 0.01 % Show Material materials with Schwefel of 0 - 0.01 % |
Silizium | 0 - 0.1 % Show Material materials with Silizium of 0 - 0.1 % |
Titan | 0.5 - 0.8 % Show Material materials with Titan of 0.5 - 0.8 % |
Zirkonium | 0 - 0.02 % Show Material materials with Zirkonium of 0 - 0.02 % |