Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 17 % Show Material materials with Dehnung of 17 % | |
Elastizitätsmodul | 23.0 °C | 210 GPa Show Material materials with Elastizitätsmodul of 210 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Martensitic Stainless Steel |
Schubmodule | 23.0 °C | 77 GPa Show Material materials with Schubmodule of 77 GPa | Typical for Martensitic Stainless Steel |
Streckgrenze | 23.0 °C | 400 MPa Show Material materials with Streckgrenze of 400 MPa | |
Zugfestigkeit | 23.0 °C | 630 MPa Show Material materials with Zugfestigkeit of 630 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1E-5 1/K |
Schmelzpunkt | 1450 °C Show Material materials with Schmelzpunkt of 1450 °C | |
Spezifische Wärmekapazität | 23.0 °C | 460 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 460 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 30 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 30 W/(m·K) |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
spezifischer Widerstand | 23.0 °C | 6E-7 Ω·m Show Material materials with spezifischer Widerstand of 6E-7 Ω·m | Typical for Martensitic Stainless Steel |
Chemical properties
Property | Value |
---|---|
Chrom | 12 - 14 % Show Material materials with Chrom of 12 - 14 % |
Eisen | 82.3 - 87.9 % Show Material materials with Eisen of 82.3 - 87.9 % |
Kohlenstoff | 0.15 - 0.4 % Show Material materials with Kohlenstoff of 0.15 - 0.4 % |
Mangan | 0 - 1.5 % Show Material materials with Mangan of 0 - 1.5 % |
Molybdän | 0 - 0.5 % Show Material materials with Molybdän of 0 - 0.5 % |
Nickel | 0 - 0.75 % Show Material materials with Nickel of 0 - 0.75 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |