Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9 g/cm³ Show Material materials with Dichte of 9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Zugfestigkeit | 23.0 °C | 290 MPa Show Material materials with Zugfestigkeit of 290 MPa |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K | |
Schmelzpunkt | 965 - 1100 °C Show Material materials with Schmelzpunkt of 965 - 1100 °C | Typical for Wrought Copper Pure / Low Alloyed Copper | |
Spezifische Wärmekapazität | 23.0 °C | 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 390 J/(kg·K) | |
Wärmeleitfähigkeit | 23.0 °C | 390 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 390 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | 0 - 0.1 % Show Material materials with Andere of 0 - 0.1 % |
Kupfer | 99.85 - 99.97 % Show Material materials with Kupfer of 99.85 - 99.97 % |
Silber | 0.03 - 0.05 % Show Material materials with Silber of 0.03 - 0.05 % |