Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 8.9 g/cm³ Show Material materials with Dichte of 8.9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 9.2 % Show Material materials with Dehnung of 9.2 % | |
Elastizitätsmodul | 23.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze | 23.0 °C | 240 MPa Show Material materials with Streckgrenze of 240 MPa | |
Zugfestigkeit | 23.0 °C | 300 MPa Show Material materials with Zugfestigkeit of 300 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Schmelzpunkt | 1070 °C Show Material materials with Schmelzpunkt of 1070 °C | |
Spezifische Wärmekapazität | 23.0 °C | 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 390 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 370 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 370 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Andere | 0 - 0.1 % Show Material materials with Andere of 0 - 0.1 % |
Kupfer | 99.4 - 99.8 % Show Material materials with Kupfer of 99.4 - 99.8 % |
Phosphor | 2E-3 - 5E-3 % Show Material materials with Phosphor of 2E-3 - 5E-3 % |
Schwefel | 0.2 - 0.5 % Show Material materials with Schwefel of 0.2 - 0.5 % |