Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 9 g/cm³ Show Material materials with Dichte of 9 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Elastizitätsmodul | 23.0 °C | 120 GPa Show Material materials with Elastizitätsmodul of 120 GPa | |
Poissonzahl | 23.0 °C | 0.34 [-] Show Material materials with Poissonzahl of 0.34 [-] | Typical for Wrought Copper Pure / Low Alloyed Copper |
Schubmodule | 23.0 °C | 48 GPa Show Material materials with Schubmodule of 48 GPa | Typical for Wrought Copper Pure / Low Alloyed Copper |
Streckgrenze | 23.0 °C | 320 MPa Show Material materials with Streckgrenze of 320 MPa | |
Zugfestigkeit | 23.0 °C | 360 MPa Show Material materials with Zugfestigkeit of 360 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.6E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.6E-5 1/K |
Schmelzpunkt | 1080 °C Show Material materials with Schmelzpunkt of 1080 °C | |
Spezifische Wärmekapazität | 23.0 °C | 390 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 390 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 390 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 390 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Kupfer | 99.9 - 100 % Show Material materials with Kupfer of 99.9 - 100 % |
Phosphor | 0 - 0.01 % Show Material materials with Phosphor of 0 - 0.01 % |