Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 7.8 g/cm³ Show Material materials with Dichte of 7.8 g/cm³ |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 23.0 °C | 11 - 21 % Show Material materials with Dehnung of 11 - 21 % | |
Elastizitätsmodul | 23.0 °C | 200 GPa Show Material materials with Elastizitätsmodul of 200 GPa | |
Poissonzahl | 23.0 °C | 0.3 [-] Show Material materials with Poissonzahl of 0.3 [-] | Typical for Steel |
Streckgrenze | 23.0 °C | 600 - 1260 MPa Show Material materials with Streckgrenze of 600 - 1260 MPa | |
Zugfestigkeit | 23.0 °C | 910 - 1410 MPa Show Material materials with Zugfestigkeit of 910 - 1410 MPa |
Thermisch
Property | Temperature | Value |
---|---|---|
Koeffizient der thermischen Ausdehnung | 23.0 °C | 1.3E-5 1/K Show Material materials with Koeffizient der thermischen Ausdehnung of 1.3E-5 1/K |
Schmelzpunkt | 1400 °C Show Material materials with Schmelzpunkt of 1400 °C | |
Spezifische Wärmekapazität | 23.0 °C | 500 J/(kg·K) Show Material materials with Spezifische Wärmekapazität of 500 J/(kg·K) |
Wärmeleitfähigkeit | 23.0 °C | 16 W/(m·K) Show Material materials with Wärmeleitfähigkeit of 16 W/(m·K) |
Chemical properties
Property | Value |
---|---|
Chrom | 15 - 17 % Show Material materials with Chrom of 15 - 17 % |
Eisen | 69.6 - 79 % Show Material materials with Eisen of 69.6 - 79 % |
Kohlenstoff | 0 - 0.07 % Show Material materials with Kohlenstoff of 0 - 0.07 % |
Kupfer | 3 - 5 % Show Material materials with Kupfer of 3 - 5 % |
Mangan | 0 - 1.5 % Show Material materials with Mangan of 0 - 1.5 % |
Molybdän | 0 - 0.6 % Show Material materials with Molybdän of 0 - 0.6 % |
Nickel | 3 - 5 % Show Material materials with Nickel of 3 - 5 % |
Niobium | 0 - 0.45 % Show Material materials with Niobium of 0 - 0.45 % |
Phosphor | 0 - 0.04 % Show Material materials with Phosphor of 0 - 0.04 % |
Schwefel | 0 - 0.03 % Show Material materials with Schwefel of 0 - 0.03 % |
Silizium | 0 - 1 % Show Material materials with Silizium of 0 - 1 % |