Chemical properties
Property | Value |
---|---|
Aluminium | 99.98 % Show Supplier Material materials with Aluminium of 99.98 % |
Andere | 0.002 % Show Supplier Material materials with Andere of 0.002 % |
Chrom | 0.0007 % Show Supplier Material materials with Chrom of 0.0007 % |
Eisen | 0.0046 % Show Supplier Material materials with Eisen of 0.0046 % |
Gallium | 0.0036 % Show Supplier Material materials with Gallium of 0.0036 % |
Kupfer | 0.0001 % Show Supplier Material materials with Kupfer of 0.0001 % |
Magnesium | 0.0005 % Show Supplier Material materials with Magnesium of 0.0005 % |
Mangan | 0.0012 % Show Supplier Material materials with Mangan of 0.0012 % |
Nickel | 0.001 % Show Supplier Material materials with Nickel of 0.001 % |
Silizium | 0.0074 % Show Supplier Material materials with Silizium of 0.0074 % |
Titan | 0.0001 % Show Supplier Material materials with Titan of 0.0001 % |
Vanadium | 0.0015 % Show Supplier Material materials with Vanadium of 0.0015 % |
Zink | 0.001 % Show Supplier Material materials with Zink of 0.001 % |
Technological properties
Property | ||
---|---|---|
Application areas | High Purity Aluminum / Dilution metal / Capacitor foil / Current collectors / Additive manufacturing / 3D printing / Specilaty alloys / Powder / Sapphire / Battery (Li-ion, Al-Air) | |
Delivery condtion | Available delivery forms: | |
Other | Listed chemical properties represent typical values obtained by Nature Alu. Purity adjustments can be made to meet customer needs on a case-by-case basis. |