Chemical properties
Property | Value | Comment |
---|---|---|
Aluminium | 99.998 % Show Supplier Material materials with Aluminium of 99.998 % | |
Andere | 0.0003 % Show Supplier Material materials with Andere of 0.0003 % | |
Chrom | 0.0003 % Show Supplier Material materials with Chrom of 0.0003 % | |
Eisen | 3e-05 % Show Supplier Material materials with Eisen of 3e-05 % | Less than |
Gallium | 0.0005 % Show Supplier Material materials with Gallium of 0.0005 % | |
Kupfer | 1e-05 % Show Supplier Material materials with Kupfer of 1e-05 % | Less than |
Magnesium | 2e-05 % Show Supplier Material materials with Magnesium of 2e-05 % | Less than |
Mangan | 0.0005 % Show Supplier Material materials with Mangan of 0.0005 % | |
Nickel | 2e-05 % Show Supplier Material materials with Nickel of 2e-05 % | Less than |
Silizium | 0.0007 % Show Supplier Material materials with Silizium of 0.0007 % | |
Titan | 3e-05 % Show Supplier Material materials with Titan of 3e-05 % | Less than |
Vanadium | 0.0002 % Show Supplier Material materials with Vanadium of 0.0002 % | |
Zink | 0.0003 % Show Supplier Material materials with Zink of 0.0003 % |
Technological properties
Property | ||
---|---|---|
Application areas | High Purity Aluminum / Capacitor foil / Current collectors / Additive manufacturing / 3D printing / Specilaty alloys / Powder / Sapphire / Battery (Li-ion, Al-Air) | |
Delivery condtion | Available delivery forms: | |
Other | Listed chemical properties represent typical values obtained by Nature Alu. Purity adjustments can be made to meet customer needs on a case-by-case basis. The comment "Less than" means that the value is under the OES limit of detection. |