Property | Value |
---|---|
Dichte | 8.9 g/cm³ Show Supplier Material materials with Dichte of 8.9 g/cm³ |
Abmessung
Property | Value |
---|---|
Dimensions | Strip thickness 0.08 - 3.0 mm, other gauges on request. Strip width from 8.5 mm. Electroplated and Hot-dip tinned strip available. |
Mechanisch
Property | Value | Testing Standard | Comment |
---|---|---|---|
Biegefestigkeit 180°, in longitudinaler Richtung | 1 [-] Show Supplier Material materials with Biegefestigkeit 180°, in longitudinaler Richtung of 1 [-] | ASTM B820 | R480 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
2 [-] Show Supplier Material materials with Biegefestigkeit 180°, in longitudinaler Richtung of 2 [-] | ASTM B820 | R540 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Biegefähigkeit 180°, in transversaler Richtung | 1 [-] Show Supplier Material materials with Biegefähigkeit 180°, in transversaler Richtung of 1 [-] | ASTM B820 | R480 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
2.5 [-] Show Supplier Material materials with Biegefähigkeit 180°, in transversaler Richtung of 2.5 [-] | ASTM B820 | R540 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Biegefähigkeit 90°, in longitudinaler Richtung | 0.5 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 0.5 [-] | EN ISO 7438 | R480 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Biegefähigkeit 90°, in longitudinaler Richtung of 1 [-] | EN ISO 7438 | R540 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Biegefähigkeit 90°, in transversaler Richtung | 0.5 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 0.5 [-] | EN ISO 7438 | R480 | bending thickness ≤ 0.5 mm & bending width: 10 mm |
1 [-] Show Supplier Material materials with Biegefähigkeit 90°, in transversaler Richtung of 1 [-] | EN ISO 7438 | R540 | bending thickness ≤ 0.5 mm & bending width: 10 mm | |
Dehnung | 4 % Show Supplier Material materials with Dehnung of 4 % | min. | R540, A50 | |
8 % Show Supplier Material materials with Dehnung of 8 % | min. | R480, A50 | ||
Elastizitätsmodul | 135 GPa Show Supplier Material materials with Elastizitätsmodul of 135 GPa | ||
Härte, Vickers | 150 - 190 [-] Show Supplier Material materials with Härte, Vickers of 150 - 190 [-] | R480 | For reference only | |
160 - 200 [-] Show Supplier Material materials with Härte, Vickers of 160 - 200 [-] | R540 | For reference only | ||
Poissonzahl | 0.33 [-] Show Supplier Material materials with Poissonzahl of 0.33 [-] | ||
Streckgrenze | 450 MPa Show Supplier Material materials with Streckgrenze of 450 MPa | min. | R480 | |
500 MPa Show Supplier Material materials with Streckgrenze of 500 MPa | min. | R540 | ||
Zugfestigkeit | 480 - 570 MPa Show Supplier Material materials with Zugfestigkeit of 480 - 570 MPa | R480 | |
540 - 630 MPa Show Supplier Material materials with Zugfestigkeit of 540 - 630 MPa | R540 |
Thermisch
Property | Temperature | Value | Comment |
---|---|---|---|
Koeffizient der thermischen Ausdehnung | 1.86e-05 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 1.86e-05 1/K | average value between 20-300°C | |
Spezifische Wärmekapazität | 381 J/(kg·K) Show Supplier Material materials with Spezifische Wärmekapazität of 381 J/(kg·K) | ||
Wärmeleitfähigkeit | 20 °C | 340 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 340 W/(m·K) |
Elektrisch
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Application target: Ideal for power connectors. | |
Chemical composition | The chemical composition is the nominal composition of the alloy | |
Coating | Electroplating: Average Hot dip tinning: Average | |
Cold Forming | Good | |
Machining | Not suitable | |
Packaging size | Standard coils with outside diameters up to 1200 mm. Traverse-wound coils with drum weights up to 500 kg. Multiple-coil up to 3 tons. | |
Soldering general | Soft soldering: Average | |
Testings | Fatigue strength: The fatigue strength is defined as the maximum bending stress amplitude which a material withstands for 10.000.000 load cycles under symmetrical alternate load without breaking. It depends on the temper selected and can be estimated typically by 1/3 of tensile strength. For solid solution fine grain materials fatigue strength might increase up to 0,5 * of tensile strength. Bending test: 90° bend test According to EN ISO 7438, 180° bend test acc. to ASTM B820, shown values might show orange- peel, however no crack. | |
Welding | Laser welding: Average Resistance welding: Good |