Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 17 g/cm³ Show Supplier Material materials with Dichte of 17 g/cm³ |
Mechanisch
Property | Temperature | Value |
---|---|---|
Elastizitätsmodul | 23.0 °C | 330 GPa Show Supplier Material materials with Elastizitätsmodul of 330 GPa |
Chemical properties
Property | Value |
---|---|
Kupfer | binder |
Nickel | binder |
Wolfram | 90 % Show Supplier Material materials with Wolfram of 90 % |
Technological properties
Property | ||
---|---|---|
Application areas | Inermet® tungsten alloys are distinguished by their particularly high density. Combined with their ability to absorb radiation as well as their outstanding mechanical properties and machinability, they are the ideal materials for a wide range of applications, such as in aerospace, the automotive industry, medical engineering and the construction industry. | |
Other | Paramagnetic |