Allgemein
Property | Temperature | Value |
---|---|---|
Dichte | 23.0 °C | 18.75 - 18.85 g/cm³ Show Supplier Material materials with Dichte of 18.75 - 18.85 g/cm³ |
Oberflächenrauigkeit | 1 μm Show Supplier Material materials with Oberflächenrauigkeit of 1 μm |
Abmessung
Property | Value |
---|---|
Durchmesser | 3.5 - 20 mm Show Supplier Material materials with Durchmesser of 3.5 - 20 mm |
Länge | 300 - 1600 mm Show Supplier Material materials with Länge of 300 - 1600 mm |
Dimensions | Available dimensions (diameter x length, mm x mm): 3.5 x 500-1524; 4.5 x 500-1524; 5.5 x 500-1524; 6.5 x 500-1524; 7 x 500-1524; 7.5 x 500-1524; 8.5 x 500-1524; 12.7 x 300-1524; 20 x 300-1600 |
Mechanisch
Property | Temperature | Value |
---|---|---|
Härte, Vickers, 30 | 23.0 °C | 400 - 420 [-] Show Supplier Material materials with Härte, Vickers, 30 of 400 - 420 [-] |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | 1E-4 % Show Supplier Material materials with Aluminium of 1E-4 % | ||
Andere | 0.9 - 1.1 % Show Supplier Material materials with Andere of 0.9 - 1.1 % | as La₂O₃ | |
Blei | 1E-4 % Show Supplier Material materials with Blei of 1E-4 % | ||
Cadmium | 1E-4 % Show Supplier Material materials with Cadmium of 1E-4 % | ||
Chrom | 3E-4 % Show Supplier Material materials with Chrom of 3E-4 % | ||
Eisen | 8E-4 % Show Supplier Material materials with Eisen of 8E-4 % | ||
Kalium | 1E-4 % Show Supplier Material materials with Kalium of 1E-4 % | ||
Kohlenstoff | 6E-4 % Show Supplier Material materials with Kohlenstoff of 6E-4 % | ||
Kupfer | 1E-4 % Show Supplier Material materials with Kupfer of 1E-4 % | ||
Lanthan | 0.77 - 0.94 % Show Supplier Material materials with Lanthan of 0.77 - 0.94 % | as La | |
Molybdän | 1.2E-3 % Show Supplier Material materials with Molybdän of 1.2E-3 % | ||
Nickel | 2E-4 % Show Supplier Material materials with Nickel of 2E-4 % | ||
Silizium | 1E-4 % Show Supplier Material materials with Silizium of 1E-4 % | ||
Stickstoff | 1E-4 % Show Supplier Material materials with Stickstoff of 1E-4 % | ||
Wolfram | balance |
Technological properties
Property | ||
---|---|---|
Application areas | WL is a popular choice for ion sources, lamp electrodes and welding electrodes. |