Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 0.89 g/cm³ Show Supplier Material materials with Dichte of 0.89 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 623 % Show Supplier Material materials with Dehnung of 623 % | ASTM D412 |
Härte, Shore A | 20.0 °C | 10 [-] Show Supplier Material materials with Härte, Shore A of 10 [-] | ASTM D2240 |
Modul bei 100 % Dehnung | 20.0 °C | 0.5 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.5 GPa | ASTM D412 |
Reißfestigkeit | 20.0 °C | 5.78 kN/m Show Supplier Material materials with Reißfestigkeit of 5.78 kN/m | ASTM D624 |
Zugfestigkeit | 20.0 °C | 1.6 MPa Show Supplier Material materials with Zugfestigkeit of 1.6 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Elastocon® 2810 is FDA compliant and well suited for consumer goods and industrial applications requiring non-slip/soft touch ergonomics and resilience. | |
Other | Elastocon® 2810 thermoplastic elastomer compound does not require drying. Elastocon® thermoplastic elastomers are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded onto polypropylene. | |
Processing methods | Injection molding, extrusion, blow molding. |