Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 0.95 g/cm³ Show Supplier Material materials with Dichte of 0.95 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 345 % Show Supplier Material materials with Dehnung of 345 % | ASTM D412 |
Härte, Shore A | 20.0 °C | 50 [-] Show Supplier Material materials with Härte, Shore A of 50 [-] | ASTM D2240 |
Modul bei 100 % Dehnung | 20.0 °C | 1.9 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 1.9 GPa | ASTM D412 |
Reißfestigkeit | 20.0 °C | 22.1 kN/m Show Supplier Material materials with Reißfestigkeit of 22.1 kN/m | ASTM D624 |
Zugfestigkeit | 20.0 °C | 3.4 MPa Show Supplier Material materials with Zugfestigkeit of 3.4 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Elastocon® 3353 is heat sealable and well suited for consumer goods and extruded tubing and profile applications. | |
Other | Elastocon® 3353 thermoplastic elastomer compound does not require drying. Elastocon® concentrates are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded and/or coextruded onto polystyrene. | |
Processing methods | Injection molding, extrusion. |