Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Dichte | 20.0 °C | 0.88 g/cm³ Show Supplier Material materials with Dichte of 0.88 g/cm³ | ASTM D792 |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dehnung | 20.0 °C | 543 % Show Supplier Material materials with Dehnung of 543 % | ASTM D412 |
Härte, Shore A | 20.0 °C | 25 [-] Show Supplier Material materials with Härte, Shore A of 25 [-] | ASTM D2240 |
Modul bei 100 % Dehnung | 20.0 °C | 0.74 GPa Show Supplier Material materials with Modul bei 100 % Dehnung of 0.74 GPa | ASTM D412 |
Reißfestigkeit | 20.0 °C | 9.82 kN/m Show Supplier Material materials with Reißfestigkeit of 9.82 kN/m | ASTM D624 |
Zugfestigkeit | 20.0 °C | 2.4 MPa Show Supplier Material materials with Zugfestigkeit of 2.4 MPa | ASTM D412 |
Technological properties
Property | ||
---|---|---|
Application areas | Elastocon® 2825PE is FDA compliant and well suited for consumer goods and industrial applications requiring UV stability. | |
Other | Elastocon® 2825PE thermoplastic elastomer compound does not require drying. Elastocon® thermoplastic elastomers are not compatible with flexible PVC and should not be blended with or used in an application where direct contact is intended. It can be overmolded and coextruded with polyethylene. | |
Processing methods | Injection molding, extrusion, blow molding. |