Allgemein
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Dichte | 1.37 g/cm³ Show Supplier Material materials with Dichte of 1.37 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 2 % Show Supplier Material materials with Moisture absorption of 2 % | 50%RH | ISO 62 | 2 mm | |
Wasserabsorption | 7 % Show Supplier Material materials with Wasserabsorption of 7 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanisch
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Biegefestigkeit | 135 MPa Show Supplier Material materials with Biegefestigkeit of 135 MPa | 50%RH | ISO 178 | 2mm/min | |
210 MPa Show Supplier Material materials with Biegefestigkeit of 210 MPa | dry | ISO 178 | 2mm/min | ||
Biegemodul | 4.7 GPa Show Supplier Material materials with Biegemodul of 4.7 GPa | 50%RH | ISO 178 | 2mm/min | |
8.4 GPa Show Supplier Material materials with Biegemodul of 8.4 GPa | dry | ISO 178 | 2mm/min | ||
Dehnung | 2.6 % Show Supplier Material materials with Dehnung of 2.6 % | dry | ISO 527-2/1A | 5mm/min | |
3.6 % Show Supplier Material materials with Dehnung of 3.6 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Elastizitätsmodul | 5.4 GPa Show Supplier Material materials with Elastizitätsmodul of 5.4 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
9.3 GPa Show Supplier Material materials with Elastizitätsmodul of 9.3 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Schlagfestigkeit, Charpy gekerbt | 23 °C | 8 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 8 kJ/m² | dry | ISO 179/1eA | |
23 °C | 12 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 12 kJ/m² | 50%RH | ISO 179/1eA | ||
Schlagzähigkeit, Charpy ungekerbt | 55 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 55 kJ/m² | dry | ISO 179/1eU | 23°C | |
70 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Charpy ungekerbt of 70 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Zugfestigkeit | 85 MPa Show Supplier Material materials with Zugfestigkeit of 85 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
135 MPa Show Supplier Material materials with Zugfestigkeit of 135 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermisch
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Schmelzpunkt | 220 °C Show Supplier Material materials with Schmelzpunkt of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Wärmeformbeständigkeitstemperatur | 190 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 190 °C | ISO 75/2Af | 1.80 MPa | ||
215 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 215 °C | ISO 75/2Bf | 0.45 MPa | |||
Entflammbarkeit | Thickness tested (mm): 0.8, Class: HB, Standard: UL 94 |
Elektrisch
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |