Biegemodul: 4.7 GPa

Quick Comparison

Polyamide 66 (PA66)

Zytel® 79G13L NC010

Polyamide 46 (PA46)

Stanyl® TW200F6

Geliefert von:

DSM Engineering Materials

Polyamide 66 (PA66)

Zytel® 79G13HSL NC010

Polybutylenterephthalat (PBT)

Crastin® HR5315HF NC010

Polyamide 4T (PA4T)

ForTii® Ace MX53T

Geliefert von:

DSM Engineering Materials

Polybutylenterephthalat (PBT)

Crastin® HR5315HF BK503

Polyamide 4T (PA4T)

ForTii® Ace WX51-FC

Geliefert von:

DSM Engineering Materials

Polyamide 6 (PA6)

EPLAMID 6 GFI 20 NC Q1C0B501 (PA6)

Geliefert von:

EPSAN

Polyamide 66 (PA66)

Akulon® SafeConnect SC22

Geliefert von:

DSM Engineering Materials

Polycarbonat (PC)

LNP™ THERMOCOMP™ Compound DX13006

Geliefert von:

Sabic

Polypropylen (PP)

LNP™ THERMOTUF™ Compound MF0049I

Geliefert von:

Sabic

Duroplast-Polymer-matrix-verbundwerkstoff

Phenolic BT45NPM - Tube

Geliefert von:

Norplex-Micarta

Duroplast-Polymer-matrix-verbundwerkstoff

Phenolic RT193PM - Tube

Geliefert von:

Norplex-Micarta

Polyetheretherketon (PEEK)

LNP™ THERMOCOMP™ Compound LF002 - Americas

Geliefert von:

Sabic

Polypropylen (PP)

ALFACOM® 30CRL

Geliefert von:

Green World Compounding

Polypropylen (PP)

ALFACOM® 30CRH

Geliefert von:

Green World Compounding