Allgemein
Property | Value |
---|---|
Kohlenstoffbilanz | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Abmessung
Property | Value |
---|---|
Dimensions | 9,5 mm, 12 mm, 15 mm, 19 mm, 25 mm |
Mechanisch
Property | Temperature | Value |
---|---|---|
Zugfestigkeit | 23.0 °C | 115 - 130 MPa Show Supplier Material materials with Zugfestigkeit of 115 - 130 MPa |
Thermisch
Property | Value | Comment |
---|---|---|
Schmelzpunkt | 660 °C Show Supplier Material materials with Schmelzpunkt of 660 °C | approximate |
Elektrisch
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 61.6 % IACS Show Supplier Material materials with Specific Electrical conductivity of 61.6 % IACS | min |
Chemical properties
Technological properties
Property | ||
---|---|---|
Application areas | Electric conductors and cables | |
Processing history | Smelters: Irkutsk Aluminium Smelter (IrKAZ), Kandalaksha Aluminium Smelter (KAZ) |