Allgemein
Property | Value |
---|---|
Kohlenstoffbilanz | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Abmessung
Property | Value |
---|---|
Dimensions | 9,5 mm |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Zugfestigkeit | 23.0 °C | 110 MPa Show Supplier Material materials with Zugfestigkeit of 110 MPa | min |
Elektrisch
Property | Value | Comment |
---|---|---|
Specific Electrical conductivity | 60.5 % IACS Show Supplier Material materials with Specific Electrical conductivity of 60.5 % IACS | min |
Chemical properties
Property | Value |
---|---|
Aluminium | Balance |
Eisen | 0.25 % Show Supplier Material materials with Eisen of 0.25 % |
Silizium | 0.08 % Show Supplier Material materials with Silizium of 0.08 % |
Zirkonium | 0.15 - 0.4 % Show Supplier Material materials with Zirkonium of 0.15 - 0.4 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thermal resistant electric conductors | |
Processing history | Smelters: Irkutsk Aluminium Smelter (IrKAZ) |