Allgemein
Property | Value |
---|---|
Kohlenstoffbilanz | Scope 1&2 (direct and indirect smelter emissions) - less than 4 T CO₂ eq/ T Al, average 2,6 T CO₂ eq / T Al. Total carbon footprint from cradle to gate is less than 8 T CO₂ eq / T Al. |
Abmessung
Property | Value |
---|---|
Dimensions | Cross section: 500x2130 mm, 560x1100 mm, 560x1230 mm, 560x1310 mm |
Chemical properties
Property | Value | Comment | |
---|---|---|---|
Aluminium | Balance | ||
Andere | 0.05 - 0.15 % Show Supplier Material materials with Andere of 0.05 - 0.15 % | according to DIN EN 573-3 | |
Chrom | 0.1 % Show Supplier Material materials with Chrom of 0.1 % | according to DIN EN 573-3 | |
Eisen | 0.35 % Show Supplier Material materials with Eisen of 0.35 % | according to DIN EN 573-3 | |
Kupfer | 0.15 % Show Supplier Material materials with Kupfer of 0.15 % | according to DIN EN 573-3 | |
Magnesium | 4 - 5 % Show Supplier Material materials with Magnesium of 4 - 5 % | according to DIN EN 573-3 | |
Mangan | 0.2 - 0.5 % Show Supplier Material materials with Mangan of 0.2 - 0.5 % | according to DIN EN 573-3 | |
Silizium | 0.2 % Show Supplier Material materials with Silizium of 0.2 % | according to DIN EN 573-3 | |
Titan | 0.1 % Show Supplier Material materials with Titan of 0.1 % | according to DIN EN 573-3 | |
Zink | 0.25 % Show Supplier Material materials with Zink of 0.25 % | according to DIN EN 573-3 |
Technological properties
Property | ||
---|---|---|
Application areas | Aluminium can end | |
Processing history | Smelters: Bratsk Aluminium Smelter (BrAZ) |