Allgemein
Property | Temperature | Value | Comment |
---|---|---|---|
Relative Dichte | 23.0 °C | 1.13 [-] Show Supplier Material materials with Relative Dichte of 1.13 [-] | ASTM D 792 | |
Sauerstoffindex | 23.0 °C | 39 % Show Supplier Material materials with Sauerstoffindex of 39 % | |
Wasserabsorption | 23.0 °C | 0.08 % Show Supplier Material materials with Wasserabsorption of 0.08 % | ASTM D 570 | (23°C/24hrs) |
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 87 MPa Show Supplier Material materials with Biegefestigkeit of 87 MPa | ISO 178 | yield, 2 mm/min |
Biegemodul | 23.0 °C | 2.4 GPa Show Supplier Material materials with Biegemodul of 2.4 GPa | ISO 178 | 2 mm/min |
Dehnung | 23.0 °C | 9.2 % Show Supplier Material materials with Dehnung of 9.2 % | ISO 527 | break, 50 mm/min |
Elastizitätsmodul | 23.0 °C | 2.6 GPa Show Supplier Material materials with Elastizitätsmodul of 2.6 GPa | ISO 527 | 1 mm/min |
Hardness, Rockwell R | 23.0 °C | 120 [-] Show Supplier Material materials with Hardness, Rockwell R of 120 [-] | ASTM D 785 |
Impact strength, Izod notched, ASTM | 23.0 °C | 293 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 293 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 100 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 100 J/m | ASTM D 4812 | unnotched, -30°C |
Schlagfestigkeit, Charpy gekerbt | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Schlagfestigkeit, Charpy gekerbt of 20 kJ/m² | ISO 179/2C | 23°C |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 20 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 20 kJ/m² | ISO 180/1A | notched 80*10*4, 23°C |
Taber Abrasion | 23.0 °C | 76 mg/1000cy Show Supplier Material materials with Taber Abrasion of 76 mg/1000cy | ASTM D 1044 | CS-17, 1 kg |
Zugfestigkeit | 23.0 °C | 50 MPa Show Supplier Material materials with Zugfestigkeit of 50 MPa | ISO 527 | break, 50 mm/min |
Thermisch
Property | Temperature | Value | Comment | ||
---|---|---|---|---|---|
Glow Wire Flammability Index | 960 °C Show Supplier Material materials with Glow Wire Flammability Index of 960 °C | ||||
Glow Wire Ignition Temperature | 775 °C Show Supplier Material materials with Glow Wire Ignition Temperature of 775 °C | IEC 60695-2-13 | 2.0 mm | |||
Heat deflection temperature, 0.45 MPa | 95 °C Show Supplier Material materials with Heat deflection temperature, 0.45 MPa of 95 °C | ISO 75/Bf | Flatw 80*10*4 sp=64mm | |||
Heat deflection temperature, 1.80 MPa | 82 °C Show Supplier Material materials with Heat deflection temperature, 1.80 MPa of 82 °C | ISO 75/Af | Flatw 80*10*4 sp=64mm | |||
Koeffizient der thermischen Ausdehnung | 23.0 °C | 7.7E-5 1/K Show Supplier Material materials with Koeffizient der thermischen Ausdehnung of 7.7E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Relative temperature index, electrical | 95 °C Show Supplier Material materials with Relative temperature index, electrical of 95 °C | UL 746B | |||
Relative temperature index, mechanical impact | 80 °C Show Supplier Material materials with Relative temperature index, mechanical impact of 80 °C | UL 746B | |||
Relative temperature index, mechanical strength | 95 °C Show Supplier Material materials with Relative temperature index, mechanical strength of 95 °C | UL 746B | |||
Vicat-Erweichungstemperatur | 107 °C Show Supplier Material materials with Vicat-Erweichungstemperatur of 107 °C | ISO 306 | Rate B/120 | |||
Wärmeformbeständigkeitstemperatur | 82 - 95 °C Show Supplier Material materials with Wärmeformbeständigkeitstemperatur of 82 - 95 °C | ||||
Wärmeleitfähigkeit | 23.0 °C | 0.24 W/(m·K) Show Supplier Material materials with Wärmeleitfähigkeit of 0.24 W/(m·K) | ASTM C177 | ||
thermischer Ausdehnungskoeffizient, transversal | 23.0 °C | 8.1E-5 1/K Show Supplier Material materials with thermischer Ausdehnungskoeffizient, transversal of 8.1E-5 1/K | ASTM E 831 | -40°C to 40°C | ||
Entflammbarkeit | UL Recognized, 94V-0 Flame Class Rating: ≥1.5mm UL 94 <br> UL Recognized, 94HB Flame Class Rating: ≥1mm UL 94 <br> UL Recognized, 94-5VA Flame Class Rating: ≥3mm UL 94 <br> Glow Wire Flammability Index, 1.0 mm: 960°C IEC 60695-2-12 <br> Glow Wire Ignitability Temperature, 1.0 mm: 800°C IEC 60695-2-13 <br> UV-light, water exposure/immersion: F1- UL 746C <br> UL Yellow Card Link: https://iq.ul.com/ul/cert.aspx?ULID=100110158- - <br> UL Yellow Card Link 2: https://iq.ul.com/ul/cert.aspx?ULID=100110159- - |
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Dielectric constant, 1KHz | 23.0 °C | 2.6 [-] Show Supplier Material materials with Dielectric constant, 1KHz of 2.6 [-] | ASTM D 150 |
Dielektrizitätskonstante, 100 Hz | 23.0 °C | 2.74 [-] Show Supplier Material materials with Dielektrizitätskonstante, 100 Hz of 2.74 [-] | ASTM D 150 |
Dissipation factor, 100Hz | 23.0 °C | 0.01 [-] Show Supplier Material materials with Dissipation factor, 100Hz of 0.01 [-] | ASTM D 150 |
Dissipation factor, 100kHz | 23.0 °C | 5.5E-3 [-] Show Supplier Material materials with Dissipation factor, 100kHz of 5.5E-3 [-] | ASTM D 150 |
Durchschlagfestigkeit | 23.0 °C | 19.2 kV/mm Show Supplier Material materials with Durchschlagfestigkeit of 19.2 kV/mm | ASTM D 149 | in oil, 3.2 mm |
High Amp Arc Ignition | 23.0 °C | 6 mm Show Supplier Material materials with High Amp Arc Ignition of 6 mm | ≥, UL 746A | PLC 0 |
High Volt Arc Track Rate | 23.0 °C | 4 PLC Code Show Supplier Material materials with High Volt Arc Track Rate of 4 PLC Code | UL 746A | (PLC) |
Hot-Wire Ignition | 23.0 °C | 6 mm Show Supplier Material materials with Hot-Wire Ignition of 6 mm | ≥, UL 746A | PLC 1 |
Kriechstromfestigkeit | 23.0 °C | 1 V Show Supplier Material materials with Kriechstromfestigkeit of 1 V | UL 746A | (UL) {PLC} |
Volume resistivity | 23.0 °C | 1.80E+16 Ω·cm Show Supplier Material materials with Volume resistivity of 1.80E+16 Ω·cm | ASTM D 257 |
Rheological Properties
Property | Temperature | Value | Comment |
---|---|---|---|
Schmelzmassenflussrate | 20 g/10min Show Supplier Material materials with Schmelzmassenflussrate of 20 g/10min | ASTM D 1238 | 280°C/5.0 kgf | |
Schmelzvolumenflussrate | 23 cm³/10min Show Supplier Material materials with Schmelzvolumenflussrate of 23 cm³/10min | ISO 1133 | MVR at 280°C/5.0 kg | |
Schrumpfung | 23.0 °C | 0.5 % Show Supplier Material materials with Schrumpfung of 0.5 % | SABIC method | 3.2 mm |
Technological properties
Property | ||
---|---|---|
Application areas | Vending Machine, Swimming Pool/Spa, Wireless Communications, Wiring Devices, Wearables, Laser Sintering, Power Manangement, Photovoltaic Components, Plumbing, Photo/Video Camera, Servingware, Small Appliance, Surgical Devices, Security/Detection, Respiratory, Monitoring and Imaging, Meter Water, Medical Facility Infrastructure, LED Lighting, Medical Device, Personal Computing, Personal Care, Non-LED Lighting, Document Handling, Door Handle, Displays, Data Transfer, Data Management, Algae, Building Element, Circuit Protection, Audio, Air Conditioning, Electronic Components, Enclosures, Energy Management, Electronics, Enclosure/Housing/Cover, Lab Ware and Clinical Diagnostics, Heavy Vehicles, Wire & cable | |
Availability | Asia,Americas | |
Processing methods | Nozzle Temperature: 250 to 275.0°C | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |