Allgemein
Mechanisch
Property | Temperature | Value | Comment |
---|---|---|---|
Biegefestigkeit | 23.0 °C | 268 MPa Show Supplier Material materials with Biegefestigkeit of 268 MPa | ASTM D 790 | brk, 1.3 mm/min, 50 mm span |
Biegemodul | 23.0 °C | 9.7 GPa Show Supplier Material materials with Biegemodul of 9.7 GPa | ASTM D 790 | 1.3 mm/min, 50 mm span |
Dehnung | 23.0 °C | 2.4 % Show Supplier Material materials with Dehnung of 2.4 % | ASTM D 638 | brk, Type I, 5 mm/min |
Elastizitätsmodul | 23.0 °C | 11.2 GPa Show Supplier Material materials with Elastizitätsmodul of 11.2 GPa | ASTM D 638 | 5 mm/min |
Impact strength, Izod notched, ASTM | 23.0 °C | 69 J/m Show Supplier Material materials with Impact strength, Izod notched, ASTM of 69 J/m | ASTM D 256 | notched, 23°C |
Impact strength, Izod unnotched, ASTM | 23.0 °C | 524 J/m Show Supplier Material materials with Impact strength, Izod unnotched, ASTM of 524 J/m | ASTM D 4812 | 23°C |
Poissonzahl | 23.0 °C | 0.4 [-] Show Supplier Material materials with Poissonzahl of 0.4 [-] | ASTM E 132 |
Schlagzähigkeit, Izod gekerbt | 23.0 °C | 69 kJ/m² Show Supplier Material materials with Schlagzähigkeit, Izod gekerbt of 69 kJ/m² | ASTM D 256 | notched, 23°C |
Zugfestigkeit | 23.0 °C | 197 MPa Show Supplier Material materials with Zugfestigkeit of 197 MPa | ASTM D 638 | brk, Type I, 5 mm/min |
Thermisch
Elektrisch
Property | Temperature | Value | Comment |
---|---|---|---|
Sheet resistivity, ROA | 23.0 °C | 100000 - 1000000 Ω Show Supplier Material materials with Sheet resistivity, ROA of 100000 - 1000000 Ω | ASTM D 257 |
Technological properties
Property | ||
---|---|---|
Availability | Europe,Asia,Americas | |
Processing methods | Maximum Moisture Content: 0.02% | |
Supplier Disclaimer | While the information is provided in good faith, SABIC MAKES NO WARRANTY, EXPRESS OR IMPLIED, INCLUDING MERCHANTABILITY AND NONINFRINGEMENT OF INTELLECTUAL PROPERTY, NOR ASSUMES ANY LIABILITY, DIRECT OR INDIRECT, WITH RESPECT TO THE PERFORMANCE, SUITABILITY OR FITNESS FOR INTENDED USE OR PURPOSE OF THESE PRODUCTS IN ANY APPLICATION. Each Buyer must determine the suitability of SABIC's materials for the Buyer's particular use through appropriate testing and analysis. No statement by SABIC concerning a possible use of any product, service or design is intended, or should be construed, to grant any license under any patent or other intellectual property right. |